Title: | Deformation and strength of Ti-6Al-4V alloyed with B at cryogenic temperatures |
Authors: | Singh, Gaurav Bajargan, Govind Datta, Ranjan Ramamurty, Upadrasta |
Keywords: | Nanoscience & Nanotechnology Materials Science Metallurgy & Metallurgical Engineering Titanium Alloys Cryogenic Temperature Plastic Deformation Twinning Microstructure Refinement Cycle Fatigue Properties Cast Titanium-Alloys Mechanical-Properties Plastic-Deformation Tensile Properties Boron Addition Grain-Size 20 K Single-Crystals Pm Ti-6Al-4V |
Issue Date: | 2014 |
Publisher: | Elsevier Science Sa |
Citation: | Singh, G; Bajargan, G; Datta, R; Ramamurty, U, Deformation and strength of Ti-6Al-4V alloyed with B at cryogenic temperatures. Materials Science And Engineering A-Structural Materials Properties Microstructure And Processing 2014, 611, 45-57, http://dx.doi.org/10.1016/j.msea.2014.05.075 Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing 611 |
Abstract: | Plastic deformation and strength of Ti-6Al-4V (Ti64) alloyed with minor additions of B at cryogenic temperatures were investigated through unnotched and notched tensile tests at 20 and 77 K Marked microstructural refinement that occurs with the trace addition of B to Ti64 was exploited for examining the role of microstructural length scales on the cryogenic plastic deformation. The tensile tests were complemented with detailed microstructural characterisation using transmission electron microscopy and electron back scattered diffraction imaging of the deformed specimens. Experimental results show that the addition of 0.30 wt% and above of B to Ti64 reduces ductility, and in turn enhances the notch sensitivity to the extent that those alloys become unsuitable for low temperature applications. However, the addition of similar to 0.10 wt% B is beneficial in enhancing the low temperature strength. An examination of the yield strength variation at various temperatures reveals that at 77 K, the colony size determines the yield strength of the alloy, just as it does at room temperature; implying dislocation-mediated plasticity continues to dominate up to 77 K At 20 K however, twinning dominates the flow response, with the activation of {11 (2) over bar1} and {5 (6) over bar1 (3) over bar} twinning in addition to {10 (1) over bar2} in the base alloy resulting in enhanced ductility of it as compared to either B-modified alloys at 20 K or the base alloy itself at 77 K The observation of a reasonable correlation between the lath aspect ratio, given by the colony-to-lath thickness ratios, and yield strength variation at 20 K suggests that coarse colony size in the base alloy allows for the activation of additional twinning mechanisms. (C) 2014 Elsevier B.V. All rights reserved. |
Description: | Restricted Access |
URI: | https://libjncir.jncasr.ac.in/xmlui/10572/2461 |
ISSN: | 0921-5093 |
Appears in Collections: | Research Articles (Ranjan Datta) |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
58.pdf Restricted Access | 4.25 MB | Adobe PDF | View/Open Request a copy |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.